Physical Properties Metric English Comments
Density 1.219 g/cc
0.04404 lb/in³
ASTM D3165
Vicone High Performance Rubber VicoSeal™ 617N-BK High Performance EPDM Rubber
Two Material Product:Material 1: VicoSeal™ 617N-70 DUROMaterial 2: SS304 nitrile vulcanized to SS304 (RoHS Approved)Information provided by Vicone