Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vicone High Performance Rubber VicoSeal™ 617N-BK High Performance EPDM Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Vicone High Performance Rubber
Trade Name VicoSeal™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoSeal™ 617N-BK High Performance EPDM Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two Material Product:Material 1: VicoSeal™ 617N-70 DUROMaterial 2: SS304 nitrile vulcanized to SS304 (RoHS Approved)Information provided by Vicone
Physical Properties Metric English Comments
Density 1.219 g/cc
0.04404 lb/in³
ASTM D3165
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
75.97

@Treatment Temp. 100 °C,
Time 252000 sec
75.97

@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Tensile Strength, Yield 16.8 MPa
2440 psi
ASTM D412
15.792 MPa

@Treatment Temp. 100 °C,
Time 252000 sec
2290.4 psi

@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Elongation at Break 433.6 %
433.6 %
ASTM D412
305.86 %

@Treatment Temp. 100 °C,
Time 252000 sec
305.86 %

@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Compressive Modulus 0.000590 GPa

@Strain 5.00 %
0.0856 ksi

@Strain 5.00 %
0.00101 GPa

@Strain 10.0 %
0.146 ksi

@Strain 10.0 %
0.00159 GPa

@Strain 20.0 %
0.231 ksi

@Strain 20.0 %
0.00210 GPa

@Strain 25.0 %
0.305 ksi

@Strain 25.0 %
Compression Set 6.44 %

@Temperature 100 °C,
Time 79200 sec
6.44 %

@Temperature 212 °F,
Time 22.0 hour
ASTM D395
Descriptive Properties Value Comments
Color Black
Copyright © lookpolymers.com All Rights Reserved