Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.156 g/cc | 0.04176 lb/in³ | ASTM D792 |
North Wood Plastics PS with 40% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Density | 1.156 g/cc | 0.04176 lb/in³ | |
Dow Nordel® IP 4520 General Purpose Molding FormulationNordel® IP 4520 |