Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.02 - 1.14 g/cc | 0.0368 - 0.0411 lb/in³ | |
Lord Adhesives 18 Mix-In Accelerator for use with all Lord Acrylic Adhesives Lord Adhesives 18 Mix-In Accelerator for use with all Lord Acrylic AdhesivesLord Accelerator 18 Black Mix-In Accelerator for use with all Lord Acrylic Adhesives. May be used at ratios from 2:1 throu.. |