Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.00 g/cc | 0.0362 lb/in³ | Calculated from weight of 45 oz/sy |
Mid-Mountain Materials ARMATEX® SF45 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |