Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.001 g/cc @Temperature 15.6 °C |
0.03616 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Exxon Hyjet IV-A Exxon HyJet IV-Aplus is a fire-resistant phosphate ester hydraulic fluid designed for use in commercial aircraft. It is the best-performing Type IV fluid and offers to a great extent many of the per.. |
|||