Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4701-41-15 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Information provided by Rogers Corporation. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® Shock Seal™ 4790-79-15 Urethane Foam, Industrial Grade Thickness: 0.125"- 0.500"Color: BlackInformation provided by Rogers Corporation. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C41 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C42 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ P391SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ P392SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Hexcel® HexWeb® HDC-G-327 - 3/16 - 15.0 (R2) Heavy Density Core Designation: Material-Cell Size (inches)-DensityHexWeb® HDC is a fabric reinforced honeycomb, typically made from either fiberglass or carbon prepreg. A thermosetting node adhesive is used with eit.. |