Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.240 g/cc | 0.00867 lb/in³ | ±10%; ASTM D3574A |
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Information provided by Rogers Corporation. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C42 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
Sawbones Solid Rigid Polyurethane Foam 15 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
Zircar Ceramics Z-MAG/2300 Soluble Fiber Insulation ZIRCAR NON-RCF Insulation Type Z-MAG/2300 is a rigid combination of soluble NON-RCF silica magnesia glass fibers and inorganic binder. It is suitable for use as a substitute for insulation containin.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | ASTM D792 |
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 15 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
3M 12028 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
3M 12032 Black 3/32" (2.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
3M 12038 Black 3/8" (9.5 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Density | 0.240 - 0.260 g/cc | 0.00867 - 0.00939 lb/in³ | Free Density |
C.O.I.M. UREXTER® Lp 285 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
3M 12026 Black 1/16" (1.6 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |