Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0270 - 0.0370 g/cc | 0.000975 - 0.00134 lb/in³ | sheet density |
Zotefoams Plastazote® LD32CN Conductive Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0270 - 0.0370 g/cc | 0.000975 - 0.00134 lb/in³ | sheet density |
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0270 - 0.0360 g/cc | 0.000975 - 0.00130 lb/in³ | sheet density |
Zotefoams Plastazote® LD33FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0270 - 0.0350 g/cc | 0.000975 - 0.00126 lb/in³ | sheet density |
Zotefoams Plastazote® LD33LC Low Density Polyethylene Foam, Large Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0270 g/cc | 0.000975 lb/in³ | Core Density, ASTM D3574 |
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam, Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Density | 0.0270 - 0.0330 g/cc | 0.000975 - 0.00119 lb/in³ | |
Akzo Nobel Expancel® 091 DE 80 d30 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0270 - 0.0330 g/cc | 0.000975 - 0.00119 lb/in³ | |
Akzo Nobel Expancel® 091 DE 40 d30 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0270 - 0.0350 g/cc | 0.000975 - 0.00126 lb/in³ | sheet density |
Zotefoams Plastazote® LD34 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |