Polymer Property : Density = 0.000926 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0256 g/cc
0.000926 lb/in³
Nominal
Hexcel® HexWeb® CR III 1/4-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Density 0.0256 g/cc
0.000926 lb/in³
Nominal
Hexcel® HexWeb® CR III 3/8-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Density 0.0256 g/cc
0.000926 lb/in³
Nominal
Hexcel® HexWeb® CR III 1/4-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Density 0.0256 g/cc
0.000926 lb/in³
Nominal
Hexcel® HexWeb® CR III 3/8-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Density 0.0256 g/cc
0.000926 lb/in³
Nominal
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Density 0.0256 g/cc
0.000926 lb/in³
Nominal
Hexcel® HexWeb® CR-PAA™ 3/8-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..