Physical Properties Metric English Comments
Density 0.00900 - 0.0180 g/cc
0.000325 - 0.000650 lb/in³
Two stage pre-expansion; Usual Use
NOVA Chemicals Gedexcel® 76D Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of very low density blocks.Information provided by NOVA Chemicals.
Density 0.00900 - 0.0150 g/cc
0.000325 - 0.000542 lb/in³
Two stage pre-expansion; Usual Use
NOVA Chemicals Gedexcel® 76L Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of low density. Insulate plates with low thermal conductivity.Information provided by NOVA Chemicals.
Density 0.00900 - 0.0150 g/cc
0.000325 - 0.000542 lb/in³
Two stage pre-expansion; Usual Use
NOVA Chemicals Gedexcel® 76XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Production of low density blocks, recommended for the elastified plates after cutting..
Density 0.00900 - 0.0150 g/cc
0.000325 - 0.000542 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova T163B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for very low density foam.Applications: This grade is used mainl..
Density 0.00900 - 0.0150 g/cc
0.000325 - 0.000542 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova T263B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low density foam.Applications: This grade is used mainly for..
Density 0.00900 - 0.0140 g/cc
0.000325 - 0.000506 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova T443C Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us..