Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trade Name : SIRIUS Product List

Category Austenitic , T 300 Series Stainless Steel , Superalloy , Iron Base , T S30000 Series Stainless Steel
Manufacturer Groupe Arcelor
Tips: 50 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel Austenitic
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel Austenitic
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel Austenitic
Industeel SIRIUS 800 H+ Heat Resistant Alloy Iron Base
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel Austenitic
Industeel SIRIUS S15 Rare Earth Containing Heat Resistant Steel T S30000 Series Stainless Steel
Industeel SIRIUS 800 Heat Resistant Alloy Iron Base
Industeel SIRIUS 800 H Heat Resistant Alloy Iron Base