Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided by Aurora Technologies.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0510 lb/in³
Water Absorption 3.3 %
3.3 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 105
105
Flexural Strength 193 MPa
28000 psi
Shear Strength 103 MPa
15000 psi
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Mechanical
130 °C
266 °F
Electrical
Electrical Properties Metric English Comments
Dielectric Constant 6.7

@Frequency 1e+6 Hz
6.7

@Frequency 1e+6 Hz
Dielectric Strength 14.8 kV/mm
375 kV/in
Dielectric Breakdown 55000 V
55000 V
Dissipation Factor 0.096

@Frequency 1e+6 Hz
0.096

@Frequency 1e+6 Hz
Descriptive Properties Value Comments
Color Tan/Black/Chocolate