Colorite Polymers CS7559LS Wire and Cable Insulation Vinyl Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Colorite Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Colorite Polymers CS7559LS Wire and Cable Insulation Vinyl Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are available in UL and non-UL grades. In addition, the engineering-grade thermoplastic elastomers we offer can stand up to the most demanding applications . . . while providing the most desirable performance characteristics at a cost that’s more affordable than “ordinary” elastomers.Typical Applications: Plenum insulationInformation provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.59 g/cc
1.59 g/cc
ASTM D792
Loss On Ignition 45 %
45 %
ASTM 2863
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
10 sec; ASTM D2240
Tensile Strength, Ultimate 17.9 MPa
2600 psi
ASTM D412
Elongation at Break 205 %
205 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Brittleness Temperature -2.00 °C
28.4 °F
ASTM D746