Williams Advanced Alloys Wambraze™ WB1240 Solder

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer Williams Advanced Alloys
Trade Name Wambraze™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys Wambraze™ WB1240 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic devices. All Williams solder alloys and gold brazing alloys are available in a variety of shapes and forms, including ribbon, preform, rod, ring, wire, and custom shapes. Powders are available in select WAMBRAZE™ alloys. Trace Impurities for Brazing Alloys:C: 50 ppm maxP and Pb*: 20 ppm maxCa*, Cd*, Cs*, Li*, Mg*, Na*, Rb*, S*, Sb*, Se*, Sr*, Te*, Ti*, Zn*: each 10 ppm maxTotal* 100 ppm maxHg: None detectedInformation provided by Williams Advanced Alloys
Thermal Properties Metric English Comments
Melting Point 1200 - 1240 °C
2190 - 2260 °F
Solidus 1200 °C
2190 °F
Liquidus 1240 °C
2260 °F
Component Elements Properties Metric English Comments
Gold, Au 92 %
92 %
Palladium, Pd 8.0 %
8.0 %
Descriptive Properties Value Comments
AWS/AMS Numbers AWS BVAu-8
Compare To: Paloro