Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina 70911-35/1-HY-AC Ivory PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 70911-35/1-HY-AC Ivory PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.52 - 1.58 g/cc
1.52 - 1.58 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -1.40 - 1.6
-1.40 - 1.6
Color A, ME 12
5.29 - 8.29
5.29 - 8.29
Color B, ME 12
87.16 - 90.16
87.16 - 90.16
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92

@Time 15.0 sec
88 - 92

@Time 0.00417 hour
NBR 7456
Tensile Strength >= 10.0 MPa
>= 1450 psi
NBR NM-IEC 60811-1-1
>= 10.0 MPa
>= 1450 psi
After 168 H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
Elongation at Break >= 150 %
>= 150 %
NBR NM-IEC 60811-1-1
>= 150 %
>= 150 %
After 168H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
Thermal Properties Metric English Comments
Oxygen Index >= 30 %
>= 30 %
NBR 6245
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Maximum Variation of Elongation (%) 25
NBR NM-IEC 60811-1-2
Maximum Variation of Tensile Strength (%) 25
NBR NM-IEC 60811-1-2