Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name Portadur
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland Portadur P2 Casting Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Gold casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental
Physical Properties Metric English Comments
Density 15.3 g/cc
0.553 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 230
230
HV5/30; as cast
230
230
HV5/30; hardened
Tensile Strength, Yield 600 MPa

@Strain 0.200 %
87000 psi

@Strain 0.200 %
as cast
600 MPa

@Strain 0.200 %
87000 psi

@Strain 0.200 %
hardened
Elongation at Break 15 %
15 %
as cast
15 %
15 %
hardened
Modulus of Elasticity 98.0 GPa
14200 ksi
Component Elements Properties Metric English Comments
Copper, Cu 12.2 %
12.2 %
Gold, Au 71 %
71 %
Iridium, Ir 0.10 %
0.10 %
Palladium, Pd 1.5 %
1.5 %
Platinum, Pt 2.5 %
2.5 %
Silver, Ag 12.2 %
12.2 %
Zinc, Zn 0.50 %
0.50 %
Processing Properties Metric English Comments
Processing Temperature 699 °C
1290 °F
Preheating Temp.
Melt Temperature 888 - 932 °C
1630 - 1710 °F
Casting Temperature 1080 °C
1980 °F
Descriptive Properties Value Comments