| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Akulon® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Akulon® F160-Z PA6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | dry; ISO 1183 |
| Water Absorption | 9.5 % | 9.5 % | Sim. To ISO 62 |
| Moisture Absorption | 2.50 % | 2.50 % | Sim. To ISO 62 |
| Viscosity Test | 450 cm³/g | 450 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | dry; ISO 527-1/-2 |
| Elongation at Break | >= 50 % | >= 50 % | dry; ISO 527-1/-2 |
| Elongation at Yield | 4.0 % | 4.0 % | dry; ISO 527-1/-2 |
| Tensile Modulus | 3.20 GPa | 464 ksi | dry; ISO 527-1/-2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | dry; IEC 60093 |
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | cond; IEC 60093 |
| Dielectric Constant | 3.1 @Frequency 1.00e+6 Hz |
3.1 @Frequency 1.00e+6 Hz |
dry; IEC 60250 |
| 3.4 @Frequency 100 Hz |
3.4 @Frequency 100 Hz |
dry; IEC 60250 | |
| Dielectric Strength | 25.0 kV/mm | 635 kV/in | dry; IEC 60243-1 |
| Dissipation Factor | 0.0065 @Frequency 100 Hz |
0.0065 @Frequency 100 Hz |
dry; IEC 60250 |
| 0.0165 @Frequency 1.00e+6 Hz |
0.0165 @Frequency 1.00e+6 Hz |
dry; IEC 60250 |