| Category | Metal , Nonferrous Metal , Precious Metal , Gold Alloy |
| Manufacturer | Wieland |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Wieland 1604 Wilaform Gold.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 15.3 g/cc | 0.553 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Vickers | 150 | 150 | HV5; glowed |
| Tensile Strength, Ultimate | 550 MPa | 79800 psi | |
| Elongation at Break | 40 % | 40 % |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 870 - 890 °C | 1600 - 1630 °F | |
| Solidus | 870 °C | 1600 °F | |
| Liquidus | 890 °C | 1630 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Copper, Cu | 15 % | 15 % | |
| Gold, Au | 75 % | 75 % | |
| Other | 0.60 % | 0.60 % | |
| Silver, Ag | 9.4 % | 9.4 % |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 600.0 °C | 1112 °F | Cuvette Temp |
| Casting Temperature | 990 - 1190 °C | 1810 - 2170 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | rose 4N |