| Category | Metal , Nonferrous Metal , Copper Alloy , Precious Metal , Gold Alloy |
| Manufacturer | Wieland |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Wieland 1005 Wilaform Gold.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 11.2 g/cc | 0.405 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Vickers | 120 | 120 | HV5; glowed |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 800 - 930 °C | 1470 - 1710 °F | |
| Solidus | 800 °C | 1470 °F | |
| Liquidus | 930 °C | 1710 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Copper, Cu | 52.19 % | 52.19 % | |
| Gold, Au | 33.3 % | 33.3 % | |
| Silver, Ag | 14 % | 14 % | |
| Zinc, Zn | 0.51 % | 0.51 % |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 600.0 °C | 1112 °F | Cuvette Temp |
| Casting Temperature | 1030 - 1130 °C | 1890 - 2070 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | red |