Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® MRGF25/25 22H-GY1 Nylon 66, 25% Mineral and 25% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRGF25/25 22H-GY1 Nylon 66, 25% Mineral and 25% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
All information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ISO 527-93
Elongation at Break 2.0 %
2.0 %
ISO 527-93
Flexural Strength 190 MPa
27600 psi
ISO 178-93
Flexural Modulus 12.4 GPa
1800 ksi
ISO 178-93
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ISO 75-93