Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Manufacturer Washington Penn
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array of colors.Information provided by Washington Penn Plastic Co.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Filler Content 30 %
30 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break 125 %
125 %
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 2.10 GPa
305 ksi
1% Secant; ASTM D790
2.34 GPa
340 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Gardner Impact 18.1 J

@Temperature 23.0 °C
13.3 ft-lb

@Temperature 73.4 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
215 °F
ASTM D648