Valley Adhesives EM-220 Low Temperature Application Glue Stick

Category Polymer , Adhesive , Thermoset
Manufacturer Valley Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Valley Adhesives EM-220 Low Temperature Application Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Valley Adhesives EM-220 Low Temperature Application Glue StickBonds many plastics, polyolefins and light weight heat sensitive materials.
Physical Properties Metric English Comments
Viscosity 7100 cP
7100 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
Tensile Strength, Ultimate 2.88 MPa
417 psi
Elongation at Break 80 %
80 %
Shear Strength 3.11 MPa
451 psi
Peel Strength 2.75 kN/m
15.7 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Heat Resistance Value at 2 psi.
Softening Point 202 °C
396 °F
Processing Properties Metric English Comments
Cure Time 0.0667 min
0.00111 hour
Hot tack
Pot Life 0.33 min
0.33 min
Open Time
Descriptive Properties Value Comments
Color Opaque