Polymer Property : Vicat Softening Point = 189 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin
Features: High stiffness, high impact strength and low warpage, good top loading capability, high surface gloss.Applications: Container (tub) lids and closures.Data provided by the manufacturer.
Vicat Softening Point >= 87.0 °C
>= 189 °F
At 1 kg; ASTM D1525
Iran Petrochemical (PCC) Tabriz 6630/1 High Impact Polystyrene  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.
Vicat Softening Point 87.0 °C
189 °F
50°C/hr; 50N
Polimeri Europa SINKRAL PD H210/K ABS  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,085-25-16-25 Flame retarded (PBBE free) injection moulding grade, rated UL94-5V at 3.2 mm thick and UL 94V-0 at..
Vicat Softening Point 87.0 °C
189 °F
Softening Point, R&B; ASTM E-28
ExxonMobil Escorene® LD-770 Very High Flow EVA Resin for Specialty Applications  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A relatively low viscosity ethylene vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance, at the same viscosity of..
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Huntsman PE1503 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Huntsman PE1504 EVA Film Extrusion  (discontinued **)
5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Braskem BI 818 LDPE Injection Molding Polyethylene  (discontinued **)
Applications: Injection molding; masterbatches. Information provided by Braskem
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding. Molded parts provide excellent part detail on fast production cycles. Molded parts have excellent c..
Vicat Softening Point 87.0 °C
189 °F
resin; ASTM D1525
Lotte Chemical Titan TITANLENE® LDC800YY Low density polyethylene resin
LDC800YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC800YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2..
Vicat Softening Point 87.0 °C
189 °F
B/50; ISO R306
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 87.0 °C
189 °F
B/50; ISO R306
Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR
Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries.
Vicat Softening Point 87.0 °C
189 °F
B/120; ISO R306
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR
Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries.
Vicat Softening Point 87.0 °C
189 °F
B/50; ISO R306
Samsung Cheil Industries Starex® TX-0520 TRABS, Unreinforced
Information provided by Samsung Cheil Industries.
Vicat Softening Point 87.0 °C
189 °F
B/50; ISO R306
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 87.0 °C
189 °F
B/120; ISO R306
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR
Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries.
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
UBE J2522 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Vicat Softening Point 87.0 °C

@Load 5.10 kg
189 °F

@Load 11.2 lb
50°C per hour; ISO 306B50
Total PS CPDS 807 Flame Retardant Polystyrene
POLYSTYRENE (PS) COMPOUND (CPDS) 807 is a high impact flame retardant polystyrene for use in HGW applications. PS CPDS 807 can be supplied in both natural and colored forms.Main Characteristics:DBD..
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
UBE UMERIT 613A Metallocene LLDPE
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert..
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Eastman Tenite 307E4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t..
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade
Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give ..
Vicat Softening Point 87.0 °C
189 °F
Condition B (50N); ASTM D1525
Chevron Phillips K-Resin® KR05 Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Finished products have excellent clarity, good toughness, good s..
Vicat Softening Point 87.2 °C
189 °F
ASTM D1525
ExxonMobil LD 334.57 Clear, High Impact Film Resin
LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Dow 4010 Low Density Polyethylene (LDPE)
Polyethylene 4010 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry and moist foods packaging, sugar pouches, lidding stoc..
Vicat Softening Point 87.0 °C
189 °F
50°C/hr; 50N
Arkema Group Evatane® 1005 VN 2 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process.Applications Grade for transparent and resistant film production. Examples: curtain stretch, coextrusion, stretch hood.ISO data provided by the ma..
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
C.O.I.M. LARIPUR® LPR9060EM PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Vicat Softening Point 87.0 °C
189 °F
JIS-K-6740
Denka VINYKON R3102 PVC, R grade for hard extrusion
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Vicat Softening Point 87.0 °C
189 °F
10N; ISO 306A50
Total Lacqrene® 4801  (discontinued **)
LACQRENE® 4801 is an easy flowing, high impact polystyrene for injection molding. The very good processing characteristics of this grade allows for the production of thin articles with long flow p..
Vicat Softening Point 87.0 °C
189 °F
50 °C/h 50N; ISO 306
DSM Arnitel® CM622 TPC-ES
60 Shore D, Extrusion