Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PSI 845E Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Total Atofina
Trade Name PSI
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSI 845E Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polystyrene 845E is a high impact polystyrene specially designed for the custom sheet market. The polymer produces tough, ductile sheet with a rich matte finish. This material is especially suitable for printing and thermoforming applications.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
ASTM D638
Elongation at Yield 55 %
55 %
ASTM D638
Tensile Modulus 1.93 GPa
280 ksi
ASTM D638
Flexural Strength 42.7 MPa
6200 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.20 ft-lb/in
ASTM D256
Falling Dart Impact 12.43 J
9.167 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 91.7 °C
197 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 96.7 °C
206 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 63 %
63 %
60°; ASTM D523