Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Riblene® GM 30 R Low Density Polyethylene - Coating Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Riblene® GM 30 R Low Density Polyethylene - Coating Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Riblene GM 30 R is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 30 R is suitable for coating applications where low neck-in and high manufacturing speed are required. Moreover, for its rheological properties, Riblene GM 30 R can be used for injection molded high thickness articles, caps, closures, stoppers and houseware.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.923 g/cc
0.923 g/cc
ISO 1183
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 48
48
ISO 868/A
Tensile Strength at Break 13.0 MPa
1890 psi
ISO 527
Tensile Strength, Yield 11.0 MPa
1600 psi
ISO 527
Elongation at Break 450 %
450 %
ISO 527
Thermal Properties Metric English Comments
Melting Point 113 °C
235 °F
Internal method
Vicat Softening Point 94.0 °C

@Load 1.00 kg
201 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved