DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior package characteristics, and a tough, durable wrap are required. Excellent shrinkage and seal strength are obtained under a wide range of operating conditions.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.570 cc-mm/m²-24hr-atm
1.45 cc-mil/100 in²-24hr-atm
ASTM 1249
Water Vapor Transmission 38.0 g/m²/day
2.45 g/100 in²/day
ASTM 1249
Oxygen Transmission 165 cc-mm/m²-24hr-atm
419 cc-mil/100 in²-24hr-atm
or 11000 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 125 %
125 %
Average; ASTM D882
Modulus of Elasticity 0.260 GPa
37.7 ksi
(stiffness), ASTM D882
Impact Test 0.900 J
0.664 ft-lb
Spencer Impact ASTM D3420
Coefficient of Friction, Dynamic 0.28
0.28
ASTM D1894
Elmendorf Tear Strength MD 25 g
25 g
Orientation not specified; ASTM D1922
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ASTM D882
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
Gloss 140 %
140 %
Processing Properties Metric English Comments
Processing Temperature >= 140 °C
>= 284 °F
Wide shrink temperature range.