Total PS CPDS 819 Flame Retardant Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer Total Atofina
Trade Name PS CPDS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PS CPDS 819 Flame Retardant Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POLYSTYRENE (PS) COMPOUND (CPDS) 819 is a high impact brominated flame retardant polystyrene. A combination of high flow and high heat stability gives excellent processability and reduced cycle times. PS CPDS 819 can be supplied in both natural and colored forms.Main Characteristics:Compliant with the European ECOLABEL (2009/300/EC),DBDPE free,Excellent UV stability,High flow, high heat stability,UL94 V0 @ 1.6 mm.Applications: Covers for electrical equipment, TV covers, office automation.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity <= 1.13 g/cc
<= 1.13 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2
Elongation at Break 40 %
40 %
ISO 527-2
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
180/1A
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C

@Load 5.10 kg
185 °F

@Load 11.2 lb
50°C per hour; ISO 306B50
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Black
Processing Properties Metric English Comments
Melt Temperature <= 260 °C
<= 500 °F