Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Terraloy™ BP 18003A Thermoplastic Starch + HIPS

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Teknor Apex Company
Trade Name Terraloy™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Terraloy™ BP 18003A Thermoplastic Starch + HIPS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: Terraloy™ BP-18003A is a Thermoplastic Starch/HIPS ready-to-process compound that contains up to 30% of TPS renewable content. This compound is intended for injection molding application. Processing Method: Injection Molding Forms: Pellets Additional Information: Biobased Content: < 30.0Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.4 MPa
2520 psi
ASTM D638
Elongation at Break 17 %
17 %
ASTM D638
Tensile Modulus 1.76 GPa
255 ksi
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790B
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Users viewing this material also viewed the following: