Mechanical Properties Metric English Comments
Flexural Modulus 1.52 GPa
220 ksi
Tangent; ASTM D790
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black
Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
PolyMirae Moplen HP526N IPP/WQBF Grade Polypropylene
Moplen HP526N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP526N is a homopolymer particularly suitable for WQB (Water Quench..
Flexural Modulus 1.52 GPa
220 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CM040LN Polypropylene, Impact Copolymer, Thermoforming
COPYLENE™ CM040LN is an impact copolymer specially designed for excellent processing in thermoforming applications and is formulated with antistat and nucleation. Applications: Thermoforming, Injec..
Flexural Modulus 1.52 GPa
220 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CH043L Polypropylene, Homopolymer, Lube, Straw
COPYLENE™ CH043L is a high antistatic, medium flow polypropylene homopolymer resin, suitable for injection molding or extrusion applications. Applications: Housewares. Equivalent to Pro-fax® HL782..
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790A
BP Amoco Acclear® 8249 Random Copolymer Polypropylene, High Clarity Grade  (discontinued **)
Suggested fabrication methods: Sheet extrusion; Thermoforming; Extrusion, injection, stretch blow moldingFeatures: Ultra high clarity, Good impact, Excellent static controlComplies with FDA specific..
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
LyondellBasell Petrothene® LM600500 High Density Polyethylene
ApplicationsPETROTHENE LM 6005-00 resin is especially designed for water, milk, and juice bottles. It exhibits excellent rigidity and good processability.Regulatory StatusLM 6005-00 meets the requi..
Flexural Modulus 1.52 GPa
220 ksi
Tangent; ASTM D790
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
Flexural Modulus 1.52 GPa
220 ksi
1% Secant; ASTM D790
Flint Hills P4G4B-125A Homopolymer Polypropylene
Homopolymer, UL certified, and FDA compliant.Features: Nucleated and antistat.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills ..
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Spartech Formalloy LG Low-Gloss TPO Alloy Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Flexural Modulus 1.52 GPa
220 ksi
secant; ASTM D790
Spartech PE4325 Reinforced High Density Polyethylene Compound
Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a..
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific)
LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P701J Polypropylene Injection Molding
Key Characteristics:High stiffnessHigh glossHigh productivityGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfa..
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790B
Teknor Apex Terraloy™ BP 18003A Thermoplastic Starch + HIPS
Notes: Terraloy™ BP-18003A is a Thermoplastic Starch/HIPS ready-to-process compound that contains up to 30% of TPS renewable content. This compound is intended for injection molding application. P..
Flexural Modulus 1.52 GPa
220 ksi
Tangent; ASTM D790
Washington Penn Medium Impact Copolymer 10% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..
Flexural Modulus 1.52 GPa
220 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 5100J Blown and Cast Film Polypropylene
HomopolymerApplications: Cast and blown film applications.Formolene 5100J is a high molecular weight, highly isotactic polypropylene homopolymer designed for sheet, cast and blown film applications...
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Chase Plastics CP Pryme® PPH100-12M Polypropylene Homopolymer
Information provided by Chase Plastics.
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Clariant Renol PA1SP0004 Nylon 66, High Impact Modified, ESD
Data provided by Clariant Masterbatches
Flexural Modulus 1.52 - 2.07 GPa
220 - 300 ksi
ASTM D790
3D Systems Accura® Xtreme Plastic for SLA® Systems
For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte..
Flexural Modulus 1.52 GPa
220 ksi
0.05 in/min, 1% secant; ASTM D-790A
Braskem FF026M Homopolymer Polypropylene
Description: Excellent Color and Processing Stability, Superior Optical and Mechanical Properties, Broad Processing WindowApplications: Suggested Uses Include BOPP ApplicationsThis resin meets the r..
Flexural Modulus 1.52 GPa
220 ksi
0.05 in/min, 1% secant; ASTM D-790A
Braskem FT021NH Homopolymer Polypropylene
Description: High Clarity, Improved AppearanceApplications: Suggested Uses Include Thermoforming, Drink Cups, Deli ContainersThis resin meets the requirements for olefin polymers as defined in 21 CF..
Flexural Modulus 1.52 GPa
220 ksi
0.05 in/min, 1% secant; ASTM D-790A
Braskem TI4150WR Impact Copolymer Polypropylene
Description: Very good mold release, very high flexural modulus.Applications: Suggested uses include closures, housewares.Process: Injection Molding.This resin meets the requirements for olefin poly..
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Americas Styrenics EB6400 High Impact Polystyrene
Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it..
Flexural Modulus 1.52 GPa
220 ksi
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr..
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Asahi Kasei Thermylene® P-20TC-0736 20% Talc Filled, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 1.52 GPa
220 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CH008 Polypropylene, Homopolymer, Netting
COPYLENE™ CH008 is a fractional melt flow polypropylene homopolymer resin available in pellet form. Applications: Raffia/Tapes/Strapping; Anti-Corrosion Coating; Geotextile & Agriculture; Nets. Rep..
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet)
Flexural Modulus 1.52 GPa
220 ksi
0.05 in/min, 1% secant; ASTM D-790A
Braskem D130C Homopolymer Polypropylene
Description: High BulkApplications: Suggested Uses Include Fine Denier Staple Fiber, High Speed Fiber SpinningThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177...