Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
15 seconds; ASTM D2240
Tensile Strength, Yield 4.83 MPa
700 psi
100%; ASTM D412
15.2 MPa
2200 psi
ASTM D412
Elongation at Break 340 %
340 %
ASTM D412
Tear Strength, Total 910.2 N
204.6 lb (f)
Die C; ASTM D1004
Compression Set 16 %
16 %
73°F, 22 hr.; ASTM D395
55 %
55 %
158°F, 22 hr.; ASTM D395
60 %
60 %
212°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746