Teknor Apex Company
Trade Name Flexalloy®
Trade Name :
Flexalloy®
Product List
Category
PVC, Wire and Cable Grade
Manufacturer
Teknor Apex Company
Tips:
Up to 50 items displayed.
PRODUCT NO.
Category
Teknor Apex Flexalloy® 3500-35 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3500-40 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3500-45 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3500-50 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3500-55 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3500-60 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3500-65 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3500-70 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3500-75 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3500-75NT Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3500-80 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3501-35-NT Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3501-40-NT Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3501-45-NT Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3501-50-NT Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3501-55-NT Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3501-60-NT Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3501-65-NT Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3501-70-NT Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 3501-75-NT Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 89501-83 Polyvinyl Chloride, Elastomer
PVC, Flexible Grade
Teknor Apex Flexalloy® 89501-83FR Polyvinyl Chloride, Elastomer
PVC, Flexible Grade
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 9100-45 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 9100-55 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 9100-65 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 9300-60 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 9300-65 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 9300-75 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 9300-85 Polyvinyl Chloride Elastomer
Vinyl (PVC)
Teknor Apex Flexalloy® 9600-72 Polyvinyl Chloride, Elastomer
PVC, Flexible Grade
Teknor Apex Flexalloy® 9601-72 Polyvinyl Chloride, Elastomer
PVC, Flexible Grade
Teknor Apex Flexalloy® 9602-72 Polyvinyl Chloride, Elastomer
PVC, Flexible Grade
Teknor Apex Flexalloy® 9602-72FR Polyvinyl Chloride, Elastomer
PVC, Flexible Grade
Teknor Apex Flexalloy® 9604-75 Polyvinyl Chloride, Elastomer
PVC, Flexible Grade
Teknor Apex Flexalloy® 9606-65 Polyvinyl Chloride, Elastomer
PVC, Flexible Grade
Teknor Apex Flexalloy® 9607-96 Polyvinyl Chloride, Elastomer
PVC, Flexible Grade
Teknor Apex Flexalloy® 9609-80 Polyvinyl Chloride Compound
Vinyl (PVC)
Teknor Apex Flexalloy® 9800-40 Polyvinyl Chloride Elastomer
PVC, Wire and Cable Grade
Teknor Apex Flexalloy® 9800-45 Polyvinyl Chloride Elastomer
PVC, Wire and Cable Grade
Teknor Apex Flexalloy® 9800-50 Polyvinyl Chloride Elastomer
PVC, Wire and Cable Grade
Teknor Apex Flexalloy® 9800-55 Polyvinyl Chloride Elastomer
PVC, Wire and Cable Grade
Teknor Apex Flexalloy® 9800-60 Polyvinyl Chloride Elastomer
PVC, Wire and Cable Grade
Teknor Apex Flexalloy® 9900-40 Polyvinyl Chloride Elastomer
PVC, Wire and Cable Grade
Teknor Apex Flexalloy® 9900-45 Polyvinyl Chloride Elastomer
PVC, Wire and Cable Grade
Teknor Apex Flexalloy® 9900-60 Polyvinyl Chloride Elastomer
PVC, Wire and Cable Grade
Teknor Apex Flexalloy® 9605-70FR Polyvinyl Chloride, Elastomer
PVC, Flexible Grade