Teknor Apex APEX® 3055-H Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 3055-H Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-ExtrusionInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
15 seconds; ASTM D2240
61
61
ASTM D2240
Tensile Strength at Break 8.14 MPa
1180 psi
ASTM D412
Tensile Strength, Yield 2.55 MPa
370 psi
100%; ASTM D412
Elongation at Break 420 %
420 %
ASTM D412
Tear Strength 24.5 kN/m
140 pli
Die C; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746