Availability: North AmericaForms: PelletsFeature: Copolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Melt Flow 5.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
5.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D638
Elongation at Yield 30 %
30 %
ASTM D638
Flexural Yield Strength 20.7 MPa
3000 psi
ASTM D790
Flexural Modulus 0.689 GPa
100 ksi
ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm
100 ohm-cm
ASTM D257
Surface Resistance 1000 ohm
1000 ohm
ASTM D257