Techmer ES Statiblend® ABS FR AS BN

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Techmer ES
Trade Name Statiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® ABS FR AS BN.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and Flame RetardantInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Yield 15 %
15 %
ASTM D638
Flexural Yield Strength 41.4 MPa
6000 psi
ASTM D790
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C
192 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
165 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Surface Resistance 1.00e+6 ohm
1.00e+6 ohm
ASTM D257