Taiwan PU Corporation TPUA-760 TPU Shoe Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS
Manufacturer Taiwan PU Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPUA-760 TPU Shoe Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A PU resin for general application with excellent adhesion to all kinds of media.Features: Fast crystallization rateGood initial adhesionGood thermo toleranceCan be used alone or combined with a cross linking agentPolyester componentInformation provided by Taiwan PU Corporation.
Physical Properties Metric English Comments
Volatiles 85 %
85 %
MEK
Viscosity 1800 - 2200 cP

@Temperature 25.0 °C
1800 - 2200 cP

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Peel Strength 0.386 kN/m
2.20 pli
PVC vs. PVC, 15 minutes
0.526 kN/m
3.00 pli
PVC vs. PVC, 30 minutes
0.912 kN/m
5.20 pli
PVC vs. PVC, 24 minutes