| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
| Water Absorption | 0.70 % | 0.70 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 103 | 103 | ASTM D785 |
| Tensile Strength at Break | 62.1 MPa | 9000 psi | ASTM D638 |
| Elongation at Break | 4.3 % | 4.3 % | ASTM D638 |
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
| Compressive Strength | 68.9 MPa | 10000 psi | ASTM D695 |
| Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 82.8 µm/m-°C @Temperature 20.0 °C |
46.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |