Dymax 984-LVUF Conformal Coating

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 984-LVUF Conformal Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 984-LVUF Conformal CoatingTough, glossy, fluorescing with excellent adhesion to a variety of metal, ceramic and glass-filled epoxy surfaces. Cure Speed (fpm): 2 - 5 Cure Type: UV then Heat
Physical Properties Metric English Comments
Viscosity 400 - 12000 cP
400 - 12000 cP
Multiple viscosities available: 984 - 400 cP, 984LVUF - 150 cP, 984T - 2500 cP, 984GEL - 12,000 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.7 MPa
6200 psi
Descriptive Properties Value Comments
Cure Depth 0.015 in.