Borealis BorPEX™ HE2595 Black High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Borealis
Trade Name BorPEX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorPEX™ HE2595 Black High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation)).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BorPEX HE2595 is a black, molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for electron beam irradiation crosslinking. The stabilization package is optimized for good processability, easy crosslinking as well as service at high temperatures. Well dispersed carbon black gives outstanding UV resistance. Crosslinked pipes based on BorPEX HE2595 are recommended for domestic hot and cold water supply, natural gas distribution, radiator connection, floor heating and industrial applications.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
Base Resin; ISO 1183
0.955 g/cc
0.0345 lb/in³
Compound; ISO 1183
Carbon Black Loading 2.2 %
2.2 %
ASTM D1603
High Load Melt Index 7.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
7.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.00 MPa
2611 psi
At 50 mm/min; ISO 527-2
Elongation at Break >= 600 %
>= 600 %
ISO 527-2