Techmer ES HiFill® PA6 HS YL030 Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6 HS YL030 Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Fast Molding Cycle and Good AdhesionAppearance: YellowTPCI# 10054102Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 2.8 %

@Time 86400 sec
2.8 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Thickness 3.17 mm
0.0070 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 90.3 MPa
13100 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Strength 115 MPa
16700 psi
ASTM D790
Flexural Modulus 2.83 GPa
410 ksi
ASTM D790
Izod Impact, Notched 0.454 J/cm

@Thickness 3.17 mm
0.850 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 82.8 µm/m-°C
46.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 178 °C
352 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C
170 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Strength 18.1 kV/mm
460 kV/in
Method A (Short-Time); ASTM D149