| Category | Polymer , Thermoplastic , ABS Polymer |
| Manufacturer | Techmer ES |
| Trade Name | Electrafil® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES Electrafil® ABS-1200/SD/FR BL ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.21 g/cc | 1.21 g/cc | ASTM D792 |
| Water Absorption | 0.30 % | 0.30 % | 24 Hrs; ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 41.4 MPa | 6000 psi | ASTM D638 |
| Elongation at Break | 10 % | 10 % | ASTM D638 |
| Tensile Modulus | 2.14 GPa | 310 ksi | ASTM D638 |
| Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
| Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
| Izod Impact, Notched | 1.33 J/cm | 2.50 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
| Flammability, UL94 | V-0 @Thickness 1.59 mm |
V-0 @Thickness 0.0625 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D648 |