Sylvin Technologies 6065 LT GL 85 PVC Wire/Cable Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Sylvin Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 6065 LT GL 85 PVC Wire/Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
10 seconds
Tensile Strength, Ultimate 16.5 MPa
2400 psi
Elongation at Break 400 %
400 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air <= 105 °C
<= 221 °F
Brittleness Temperature -32.0 °C
-25.6 °F
Oxygen Index 22 %
22 %
Processing Properties Metric English Comments
Processing Temperature 166 - 177 °C
330 - 350 °F
Recommended Stock Temperature