| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Suggested Extusion Stock |
| S&E Specialty Polymers TufFlex™ GA-94-244B PVC Compound Application: 105°C rated vinyl elastomer for medical wire and cable applications. This product complies with the RoHS Directive.Information provided by S&E Specialty Polymers |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Suggested Stock |
| S&E Specialty Polymers TufTech™ G-2175A PVC Compound Application: A clear, high gloss, PVC based compound designed for profile extrusion applications.Information provided by S&E Specialty Polymers |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Suggested Stock |
| S&E Specialty Polymers TufTech™ G-2184M PVC Compound Application: A RoHS compliant, general purpose PVC based compound designed for molding applications.Information provided by S&E Specialty Polymers |
|||
| Processing Temperature | 166 - 171 °C | 330 - 340 °F | Suggested Stock |
| S&E Specialty Polymers TufTech™ GM-3958-095 PVC Compound Application: A clear, non-toxic, extrusion compound for food contact use.Information provided by S&E Specialty Polymers |
|||
| Processing Temperature | 166 - 171 °C | 330 - 340 °F | Suggested Stock |
| S&E Specialty Polymers TufTech™ GM-3968 PVC Compound Application: A clear, non-toxic, extrusion compound for food contact use.Information provided by S&E Specialty Polymers |
|||
| Processing Temperature | 166 - 171 °C | 330 - 340 °F | Suggested Stock |
| S&E Specialty Polymers TufTech™ GM-94-106D PVC Compound Application: A clear, PVC based, extrusion grade compound.Information provided by S&E Specialty Polymers |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 6161-82 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 6404-78 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 °C | 331 °F | Upper Limit Temperature |
| Spartech Polypedic A Low Density Polyethylene Description: Flexible, lower processing temperature, softApplications: Anterior shells for AFOs and KAFOs; TLSOs; passive types of HOs, WHOs and EWHOsInformation provided by Spartech. |
|||
| Processing Temperature | 166 °C | 331 °F | Upper Limit Temperature |
| Spartech Polypedic C Polypropylene Copolymer Description: Resilient in cold weather, durable, slightly less rigid than Polypedic OApplications: AFOs; MAFOs; KAFOs; AK and BK sockets; CTLSOs; TLSOs; pelvic bands and joints; pelvic girdles; Info.. |
|||
| Processing Temperature | 166 °C | 331 °F | Upper Limit Temperature |
| Spartech Polypedic F High Density Polyethylene Description: More rigid, tough, able to withstand cold temperature applicationApplications: Neck brace; splintsInformation provided by Spartech. |
|||
| Processing Temperature | 166 °C | 331 °F | Upper Limit Temperature |
| Spartech Polypedic Modified Low Density Polyethylene Description: Flexible, wider window for forming, softApplications: Anterior shells for AFOs and KAFOs; TLSOs; passive types of HOs, WHOs and EWHOs; prosthetic flexible socketsInformation provided by.. |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 50423 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 5104 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 5108 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 5117-82 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 574 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 6064 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 6065 LT GL 85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 °C | 330 °F | |
| Advanced Polymer Alloys Alcryn® 2250 UT Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
| Processing Temperature | 166 °C | 330 °F | |
| Advanced Polymer Alloys Alcryn® 2265 UT Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
| Processing Temperature | 166 °C | 330 °F | |
| Advanced Polymer Alloys Alcryn® 4670 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
| Processing Temperature | 166 °C | 330 °F | |
| Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
| Processing Temperature | 166 °C | 330 °F | |
| Advanced Polymer Alloys Alcryn® 4680 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
| Processing Temperature | 166 °C | 330 °F | |
| Advanced Polymer Alloys Alcryn® 4680 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
| Processing Temperature | 166 °C | 330 °F | |
| Advanced Polymer Alloys Alcryn® 4660 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
| Processing Temperature | 166 °C | 330 °F | |
| Advanced Polymer Alloys Alcryn® 4660 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 6134-80 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 - 177 °C | 330 - 350 °F | Recommended Stock Temperature |
| Sylvin Technologies 6149-80 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
| Processing Temperature | 166 - 240 °C | 330 - 464 °F | Average value: 209 °C Grade Count:16 |
| Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |
|||