Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, dry

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon
Manufacturer Suzhou Hipro Polymers
Trade Name Hiprolon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, dry.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hiprolon® 200 NN is a medium viscosity polyamide 10,10 with neat resin based on bio-renewable resource. It features low density, low water absorption, good cold impact resistance, good wear-resistance and flow ability. It is widely used as neat resin for compounding, general injection molding process, tubing or film extrusion, powder coating, et al.Information provided by Suzhou Hipro Polymers Co. Ltd
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption 0.70 %
0.70 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2/1A
Tensile Modulus 1.70 GPa
247 ksi
ISO 527-1/-2
Flexural Modulus 1.60 GPa
232 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 202 °C
396 °F
ISO 11357-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-1/2
Users viewing this material also viewed the following: