Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loctite® 511 Fast Curing Thread Sealant

Category Polymer , Adhesive , Thermoset
Manufacturer Loctite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 511 Fast Curing Thread Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high pressure applications, liquid thread sealants seal instantly for low pressure testing. When fully cured, they seal to the burst strength of most piping systems.Loctite® Pre-Applied Thread Sealants are dry-to-the-touch films applied to threaded fittings by fitting suppliers and process centers located throughout North America. Pre-applied thread sealants are ideal for OEMs because they can improve speed of assembly and ensure quality by eliminating on-line dispensing of sealants.Loctite® 511 Fast Curing Thread SealantA low strength, rapid fixture sealant for tapered/straight fluid fittings. Controlled strength for ease of disassembly. Seals operating pressures to 10,000 psi. Recommended Primer: 7649 (N) Typical Use: Low Strength, Rapid Fixture
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Viscosity 19000 - 60000 cP
19000 - 60000 cP
Thixotropic
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Descriptive Properties Value Comments
Color Cream