Material Notes:
Characteristics Very high clarity & gloss High dart impact strength & good stiffness Good crease retention Good heat resistance High yield compared to PVC, APET Processing Extrusion Vacuum forming Applications Blister packing Collar packs Folded clear boxes Lids Egg cartons & other rigid packaging Material Status: Commercial : ActiveAgency Ratings: FDA 21 CFR 177.1640Information provided by Supreme Petrochem LTD
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Melt Flow 6.0 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
6.0 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 36.8 MPa
5340 psi
50 mm/min; ASTM D638
Elongation at Break 10 %
10 %
50 mm/min; ASTM D638
Flexural Strength 51.5 MPa
<br>@Thickness 3.20 mm
7470 psi
<br>@Thickness 0.126 in
ASTM D790
Flexural Modulus 1.77 GPa
<br>@Thickness 3.20 mm
256 ksi
<br>@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 0.150 J/cm
<br>@Thickness 3.20 mm
0.281 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Izod Impact, Unnotched 2.75 J/cm
<br>@Thickness 3.20 mm
5.15 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
ASTM D648
Vicat Softening Point 101 °C
214 °F
1kg / 120°C; ASTM D1525
Flammability, UL94 HB
<br>@Thickness 1.60 mm
HB
<br>@Thickness 0.0630 in
Optical Properties Metric English Comments
Haze 1.5 %
<br>@Thickness 1.00 mm
1.5 %
<br>@Thickness 0.0394 in
SPL test method
Transmission, Visible 88 %
<br>@Thickness 1.00 mm
88 %
<br>@Thickness 0.0394 in
SPL test method
Processing Properties Metric English Comments
Melt Temperature <= 220 °C
<= 428 °F
Mold Temperature 40.0 - 50.0 °C
104 - 122 °F