Solvay GERONOL® TE 300 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name GERONOL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay GERONOL® TE 300 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Emulsifier for agrochemical formulations.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most polar and aromatic solventsAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: Multipurpose emulsifier.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
pH 5.0 - 7.0
5.0 - 7.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 15.0 °C
59.0 °F
Flash Point >= 61.0 °C
>= 142 °F
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Viscous liquid
Composition Active content
0.88
HLB number 10.7
Ionic Charge Anionic/Nonionic