Material Notes:
Description: DEXFLEX® D160HS is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require excellent durability, low-temperature impact resistance, low thermal expansion, and excellent weatherability. Applications: Bumper fascias, air dams, valance panels, wheel flares, bumper pads, and other components that must meet exacting dimensional tolerances. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ISO 1183
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
as molded; ISO 294
0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
after bake; ISO 294
Melt Flow 10 g/10 min
10 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 0.620 GPa
89.9 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 20.0 J
14.8 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
50.0 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228