Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Silon Taborex TA 2329 HD Catalyst Masterbatch

Category Other Engineering Material , Catalyst/Initiator
Manufacturer Silon
Trade Name Taborex
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silon Taborex TA 2329 HD Catalyst Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1117 HD. TA 2329 HD contains a cross-linking catalyst and a stabiliser package. Together with the above-mentioned grafted Polyethylene Compound TA 2329 HD Masterbatch completes a Sioplas System in white colour, approx. RAL 9001. In addition TA 2329 HD provides processing and long term stabilisation for this system.Information provided by Silon
Physical Properties Metric English Comments
Bulk Density 0.590 g/cc
0.0213 lb/in³
Density 1.09 g/cc
0.0394 lb/in³
Volatiles <= 0.25 %
<= 0.25 %
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Storage Temperature <= 25.0 °C
<= 77.0 °F
Descriptive Properties Value Comments
Color White