| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber |
| Manufacturer | Silikony Polskie |
| Trade Name | Polastosil |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Silikony Polskie Polastosil M-33 Silicone Rubber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.10 g/cc | 1.10 g/cc | Before Curing |
| Viscosity | 50000 cP | 50000 cP | Before Curing |
| Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | After Curing |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 45 | 45 | After Curing |
| Tensile Strength at Break | 3.50 MPa | 508 psi | After Curing |
| Elongation at Break | 130 % | 130 % | After Curing |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 180 °C | 356 °F |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | <= 1440 min | <= 24.0 hour | Curing |
| Pot Life | 30 min | 30 min | Curing |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | White |